HomeOwner SearchCategory Search
Standard welding procedure specification (SWPS) for gas tungsten arc welding of austenitic stainless steel (M-8), P-8, or S-8), 18 through 10 gauge, in the as-welded condition, with or without backing AWS B2.1-8-009:2002 : an American national standard
Visit USCO
hero image
Text Registration
Copyright Title

Standard welding procedure specification (SWPS) for gas tungsten arc welding of austenitic stainless steel (M-8), P-8, or S-8), 18 through 10 gauge, in the as-welded condition, with or without backing AWS B2.1-8-009:2002 : an American national standard

Status

Published

on 15 Jun 2007
Year of Creation
2002
Copyright Claimant
American Welding Society
Registration Number
TX0005859932
on 15 Jun 2007

Copyright Summary


The U.S. Copyright record (Registration Number: TX0005859932) dated 15 Jun 2007, pertains to an electronic file (eService) titled "Standard welding procedure specification (SWPS) for gas tungsten arc welding of austenitic stainless steel (M-8), P-8, or S-8), 18 through 10 gauge, in the as-welded condition, with or without backing AWS B2.1-8-009:2002 : an American national standard" created in 2002. The copyright holder is American Welding Society, known for their creative contributions in text registration. For any inquiries concerning this copyrighted material, kindly reach out to American Welding Society.

Copyright Details


Copyright Claimant
American Welding Society

Application Details


Registration Number
TX0005859932
Registration Date
6/15/2007
Year of Creation
2002
Agency Marc Code
DLC-CO
Record Status
New
Corporate Author
American Welding Society
Physical Description
12 p

Corporate Authors


Notes


Material Matter Claimed Note: New Matter: additions, revisions, compilation
Previous Registration Note: Prev. reg. 1990, TX 2-855-625